abstract |
A catalyst fibrous structure having a catalyst metal carried on a fibrous structure, wherein (a) a Log differential micropore volume distribution curve thereof obtained by measurement using a mercury intrusion technique has a peak having a maximum micropore diameter in the range of from 0.1 μm to 100 μm: (b) a Log, differential micropore volume at the peak is 0.5 mL/g or more; and (c) an amount of a catalyst metal compound and a binder carried per unit volume is 0.05 g/mL or more. Also, a production method for producing a catalyst fibrous structure. |