abstract |
A hard sheet comprising a nonwoven fabric of microfine fibers and a polymeric elastic body imparted to the nonwoven fabric is characterized in that each layer when JIS-D hardness is 45 or more and in the cross section in the thickness direction, When the first surface layer, the intermediate layer and the second surface layer were formed in this order from the side, the JIS-D hardness of the first surface layer and the intermediate layer was measured in total of 6 points each at three arbitrary points, , The ratio of R% calculated from the following formula: R (%) = (D hardness maximum value - D hardness minimum value) / D hardness average value × 100 is 0 to 20% A hard sheet having a content of 400 占 퐂 / cm3 or less. |