http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6819839-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-84 |
filingDate | 2020-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-6819839-B1 |
titleOfInvention | Exterior materials for power storage devices, their manufacturing methods, and power storage devices |
abstract | Provided is an exterior material for a power storage device, in which the matte design of the surface coating layer containing a filler is suppressed from being damaged by the heat seal, and the moldability is also excellent. From the outside, it is composed of a laminate having at least a surface coating layer, a base material layer, a barrier layer, and a thermosetting resin layer. The surface coating layer contains a resin and a filler, and contains a resin and a filler. An exterior material for a power storage device, wherein the logarithmic decrement ΔE at 200 ° C. in the rigid pendulum measurement of the outer surface of the surface coating layer of the laminated body is 0.43 or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023171807-A1 |
priorityDate | 2019-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 160.