Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 |
filingDate |
2005-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a050fb8f208c23242001f66c6e2e16d1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e3359ef092f3a3b030295377dbf6bbc |
publicationDate |
2006-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006072320-A |
titleOfInvention |
Antireflection film manufacturing method, antireflection film, polarizing plate, and image display device |
abstract |
PROBLEM TO BE SOLVED: To provide a method for producing an antireflection film having a sufficient reflection performance and excellent scratch resistance. And an antireflection film obtained by the production method. Furthermore, a polarizing plate and an image display device provided with the antireflection film are provided. A method for producing an antireflection film having an antireflection layer comprising at least one layer on a transparent substrate, wherein at least one layer on the transparent substrate comprises the following steps (1) and (2): A method for producing an antireflective film, comprising: forming a layer by a layer forming method comprising: (1) A step of coating a coating layer on a transparent substrate (2) A step of curing the coating layer by irradiating ionizing radiation in an oxygen concentration atmosphere lower than the oxygen concentration in the atmosphere. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200084862-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007283293-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102315469-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019107036-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019107036-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8206779-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I494584-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102430505-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020134941-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019171326-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9447288-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014529763-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010039418-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7071418-B2 |
priorityDate |
2004-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |