abstract |
Provided are a laminated body of acrylic resin layers, the laminated body having good impact resistance, and a method for producing the same. This laminated body comprising, in this order, a first acrylic resin layer, a thermoplastic resin layer, and a second acrylic resin layer, the thermoplastic resin layer containing at least 71% of a component taking a spin-spin relaxation time T2 H in pulse NMR measurement of at least 0.03 ms. This method for producing a laminated body comprises a step for discharging a molten resin laminated body from a die, the molten resin laminated body comprising at least a melt of a resin composition (1) containing a (meth)acrylic resin, a melt of a resin composition containing a thermoplastic resin, and a melt of a resin composition (2) containing a (meth)acrylic resin, and a step for cooling the discharged molten resin laminated body so as to obtain the laminated body. |