http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020202932-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-05 |
filingDate | 2020-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c2feb12274d897d17b1ad0415b5e13c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_051fce97d237e88f83f8856f0e405e2e |
publicationDate | 2020-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2020202932-A1 |
titleOfInvention | Addition-curable silicone adhesive composition |
abstract | This composition comprises: (A) one or both of (i) and (ii), said (i) being polysiloxane (1) having a viscosity of 50-10,000,000 mPa∙s, R2R1 2SiO(R1 2SiO)mSiR1 2R2 (1), and said (ii) being polysiloxane (2), (R1 3SiO1/2)p(R2 aR1 3-aSiO1/2)q(SiO4/2)r (2); (B) hydrogen polysiloxane (3), (HbR1 3-bSiO1/2)s(R1 3SiO1/2)2-s(HR1 1SiO2/2)t(R1 2SiO2/2)u (3); (C) a hydrosilylation catalyst; and (D) at least one among linear organosiloxane (4), (AcR3 3-cSiO1/2)v(R3 3SiO1/2)2-v(AR3 1SiO2/2)w(R3 2SiO2/2)x (4), and cyclic organopolysiloxane (5), (AR3 1SiO2/2)y(R3 2SiO2/2)z (5) (A is an alicyclic epoxy group represented by formula (6)), wherein the ratio of the total number of SiH's to the number of unsaturated bonds between (D) and the alkenyl of (A) is 0.8-1.5, said composition is rapidly cured at room temperature after mixing to exhibit adhesiveness to a substrate such as a metal or resin, and even after the cured product following adhesion is exposed to a high-temperature and high-humidity environment, the adhesiveness to the substrate does not deteriorate. |