http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020128283-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f506d01d7c64b8a38040974fa9a16821 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0052 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-02 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-12 |
filingDate | 2019-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c838e19cf974975006d7b18a98c426e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e0f7c4600ac40f47b85e12d22baaadf |
publicationDate | 2020-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2020128283-A1 |
titleOfInvention | Use of linear diols for the production of biosourced polyester foams |
abstract | The invention relates to a process for the production of a thermoset polyester foam, comprising the following steps in succession: (a) heating an essentially anhydrous pre-oligomerisation composition containing - a polyol component which contains at least 70% by weight, preferably at least 80% by weight, of a mixture of at least one hydrogenated sugar and at least one diol selected from the C 3-6 diols, - a polyacid component containing a porogenic polyacid, preferably citric acid, and optionally - a catalyst, at a temperature between 100°C and less than 160°C for between 10 and 60 minutes, preferably between 15 and 40 minutes, under mechanical agitation, so as to cause the polyol component to react with the polyacid component and form a composition of oligomeric esters, (b) incorporating a surfactant composition into the oligomeric ester composition so as to obtain a thermosetting expandable composition, (c) introducing the thermosetting expandable composition that was obtained into a mould or applying said thermosetting expandable composition to a substrate, and (d) heating the thermosetting expandable composition to a temperature at least equal to 165°C in order to form a thermoset polyester foam. |