http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3075208-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f506d01d7c64b8a38040974fa9a16821 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0023 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-12 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G101-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C67-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-02 |
filingDate | 2017-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e0f7c4600ac40f47b85e12d22baaadf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c838e19cf974975006d7b18a98c426e8 |
publicationDate | 2019-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | FR-3075208-A1 |
titleOfInvention | PROCESS FOR MANUFACTURING POLYESTER THERMODURCAL FOAMS WITH PRE-IMPROVEMENT STEP |
abstract | Method for manufacturing a thermoset polyester foam, comprising the following successive steps:n (a) heating an essentially anhydrous pre-oligomerization composition containingn - a polyol component comprising at least 30% by weight of hydrogenated sugar,n a polyacid component comprising a porogenic polyacid, preferably citric acid, andn - a catalyst,n at a temperature between 100 ° C and less than 160 ° C for a time between 10 and 60 minutes, preferably between 15 and 40 minutes, with mechanical stirring, so as to react the polyol component with the polyacid component and at form a composition of oligomeric esters,n (b) incorporation of a surfactant composition into the composition of oligomeric esters, so as to obtain an expandable thermosetting composition,n (c) introduction of the thermosetting expandable composition obtained in a mold or application of the thermosetting expandable composition on a support,n (d) heating the thermosetting expandable composition to a temperature at least equal to 160 ° C so as to form a thermoset polyester foam. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020128283-A1 |
priorityDate | 2017-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.