Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee1c19da359446fb5c4f0458a57b783d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2204-08 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C23-0075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C21-002 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1333 |
filingDate |
2016-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46f7d271928483a0e496777fde27131d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fe866d0319b94ff1b6a6f200c65fa6b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dede2c17c1958fead2d87d7a3309d6e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb67185984caa7b977823416eb59de65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53a8fffaa1887c21f6f73e3c2d246284 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1a974f23fce6f5f5b97ca52abd6d37f1 |
publicationDate |
2016-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2016117474-A1 |
titleOfInvention |
Chemically strengthened glass and production method for chemically strengthened glass |
abstract |
The purpose of the present invention is to provide a high-transmittance (i.e., low-reflectivity) chemically strengthened glass for which reduction in the strength of the glass can be effectively suppressed, even when chemical strengthening is performed. The present invention relates to a chemically strengthened glass that has, in a surface layer thereof, a compressive stress layer that is formed by means of an ion exchange method. The chemically strengthened glass includes sodium and boron and has a delta transmittance of +0.1% or more. A straight line that linearly approximates the hydrogen concentration Y at a depth X from the outermost surface of the glass satisfies a specific relational expression for X = 0.1-0.4 μm. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7056652-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018199045-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019085276-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7310966-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7031230-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018199045-A1 |
priorityDate |
2015-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |