Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c16d2144a81bfa32a665dca1e93c3d37 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-181 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7729 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7721 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7706 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-77348 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J1-63 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-00 |
filingDate |
2013-02-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b452aeb0cec2f491f82f0b5277f48b88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90986568f5405cdd9e6898177892a9af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74203eab60fa977cc4d91aded425619e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a82074fd60da460dc4d1336d66d3535e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e67b58b5c4b193a4ef0a54269e9bb81 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17396fa7df62db0e250f21bf5302b7e6 |
publicationDate |
2014-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8709838-B2 |
titleOfInvention |
Method for preparing a β-SiAlON phosphor |
abstract |
There is provided a method for preparing a β-SiAlON phosphor capable of be controlled to show characteristics such as high brightness and desired particle size distribution. The method for preparing a β-SiAlON phosphor represented by Formula: Si (6-x) Al x O y N (8-y) :Ln z (wherein, Ln is a rare earth element, and the following requirements are satisfied: 0<x≦4.2, 0<y≦4.2, and 0<z≦1.0) includes: mixing starting materials to prepare a raw material mixture; and heating the raw material mixture in a nitrogen-containing atmospheric gas, wherein the starting materials includes a host raw material including a silicon raw material including metallic silicon, and at least one aluminum raw material selected from the group consisting of metallic aluminum and aluminum compound, and at least activator raw material selected from the rare earth elements for activating the host raw material. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9559271-B2 |
priorityDate |
2008-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |