Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6394c3e374cdad0d4ba7e87fe85f73ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1183f3a7320c1b753ef3d52edb720007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_631680c9a2741e2207756e858689b3d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5520dd38cc403678d9f91e0b0ee95fb |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09392 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09357 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09307 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09371 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09314 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-09321 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-093 |
filingDate |
2007-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2011-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df474abba4ee2733ef6684933b1e0bff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a79a072cacade822d3be0e2b85c36ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_712913458f06d82da70c7399d3657bfb |
publicationDate |
2011-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8067143-B2 |
titleOfInvention |
Functional particle and manufacturing method thereof |
abstract |
A functional particle is manufactured by a method including an aggregating step, a depressurizing step, and a cooling step. In the aggregating step, the functional particle is obtained by flowing a mixed slurry containing a core particle and a shell particle through a coiled pipeline while heating the mixed slurry to a glass transition temperature or higher of the core particle, to deposit the shell particles on the surface of the core particle. In the depressurizing step, the grain size of the functional particle is controlled and the coarse particle is pulverized to make the grain size of the functional particles uniform. In the cooling step, re-aggregation of the functional particles with unified grain size is prevented. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010021210-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010009281-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8252501-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8227167-B2 |
priorityDate |
2006-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |