Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5397fc5ff75ee49a454558b68b36baa |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31612 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31938 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31935 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31855 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D1-185 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-10 |
filingDate |
2004-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2007-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9395a2cdff69a7c97c991972043f179 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60487687ac8883b5a19abaf1f6ae8acf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3765391f0f2280c001c513f3c43958d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de3dd88c6331f58dd052c79661a7036c |
publicationDate |
2007-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-7252862-B2 |
titleOfInvention |
Increasing adhesion in an imprinting procedure |
abstract |
A method for increasing adhesion between a substrate and a polymeric imprintable material during an imprinting procedure. The method includes chemically bonding a plurality of molecules to a surface of a substrate to form a self-assembled monolayer thereon. A monomer is copolymerized with the self-assembled monolayer to form a polymeric imprintable material that is chemically bonded to the self-assembled monolayer. Adhesion between the polymeric imprintable material and the substrate is substantially increased by the self-assembled monolayer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8986488-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8329089-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9293328-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014120268-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8728714-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2007246441-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I482201-B |
priorityDate |
2004-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |