abstract |
A process and composition for transforming perfluoroalkanes in the presence of an oxidizing agent and water at temperatures between about 400 to 1,000° C. Aluminum oxide is the primary agent for effecting this transformation. Additions of between 0.1 to 50% by weight of other components such as barium calcium, phosphorus, cerium, chromium, cobalt, iron, lanthanum, magnesium, nickel, silicon, titanium, yttrium or zirconium aid in extending the useful life of the catalyst. A preferred catalyst composition includes aluminum oxide with additions of cobalt and one or more of the elements of cerium, titanium or zirconium. |