An embodiment of the instant invention is a method of forming a dielectric layer, the method comprising the steps of: providing a semiconductor substrate (substrate 12), the substrate having a surface; forming an oxygen-containing layer (layer 14) on the semiconductor substrate; and subjecting the oxygen-containing layer to a nitrogen containing plasma (plasma 16) so that the nitrogen is either incorporated into the oxygen-containing layer (see regions 18, 19, and 20) or forms a nitride layer at the surface of the substrate (region 22). Using this embodiment of the instant invention, the dielectric layer can be substantially free of hydrogen. Preferably, the oxygen-containing layer is an SiO 2 layer or it is comprised of oxygen and nitrogen (preferably an oxynitride layer). The plasma is, preferably, a high-density plasma. Preferably, a source of nitrogen is introduced to the plasma to form the nitrogen containing plasma. The source of nitrogen is preferably comprised of a material consisting of: N 2 , NH 3 , NO, N 2 O, or a mixture thereof. |