abstract |
PCT No. PCT/BE93/00026 Sec. 371 Date Jan. 19, 1995 Sec. 102(e) Date Jan. 19, 1995 PCT Filed May 19, 1993 PCT Pub. No. WO93/23237 PCT Pub. Date Nov. 25, 1993In the method according to the invention, a layer of polyurethane elastomer for obtaining a polyurethane skin (5) is produced, in a first step, against a mould surface (1). In a second step, a reaction mixture for obtaining a polyurethane foam layer (6) is applied against this polyurethane skin (5). In a third step, a suitable polyurethane or polyisocyanurate reaction mixture for obtaining a rigid synthetic carrier (8) is applied against the polyurethane foam layer (6). In this way, a synthetic trim part is obtained which is easier to recycle. This method can moreover also be performed easier. |