abstract |
The present invention makes it possible to provide a semiconductor element cleaning method that is characterized in that: a hard mask pattern is formed on a substrate that has a low relative permittivity film and at least one of a cobalt, a cobalt alloy, or a tungsten plug; and a cleaning liquid that contains 0.001-20% by mass of an alkali metallic compound, 0.1-30% by mass of quaternary ammonium hydroxide, 0.01-60% by mass of a organic water-soluble solvent, 0.0001-0.1% by mass of hydrogen peroxide, and water is subsequently used on a semiconductor element in which, using the hard mask pattern as a mask, the hard mask, the low relative permittivity film, and a barrier insulating film are dry etched, and dry etch residues are removed. |