Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33034d7d450ca12d013db67b659c9088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_120a97c733cfccbe04b1298469660136 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1462 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2433-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2221-68327 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2221-68381 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-326 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-6836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-48 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-12 |
filingDate |
2011-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7991db14f7d5b502389e9a8a94d66581 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87b2aacf696bc8506109087c66c5b330 |
publicationDate |
2012-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2012291944-A1 |
titleOfInvention |
Method of producing electronic component |
abstract |
There is provided a method of producing an electronic component capable of preventing electrostatic destruction on a circuit or the like formed on the electronic component by eliminating the electrification charge generated on a pressure-sensitive adhesive sheet efficiently in a short period of time upon producing the electronic component using the pressure-sensitive adhesive sheet. The present invention is a method of producing an electronic component using a pressure-sensitive adhesive sheet in which at least a pressure-sensitive adhesive layer and a separator are sequentially stacked on a base material, the pressure-sensitive adhesive sheet having 900 seconds or less of a half-value period of the electrification charge generated on a surface of said pressure-sensitive adhesive layer by the charge decay measuring method based on JIS L1094, at least comprising: a step of peeling said separator off from said pressure-sensitive adhesive layer; a step of eliminating the electrification charge on the surface of said pressure-sensitive adhesive layer; and a step of bonding an electronic component onto said pressure-sensitive adhesive layer after charge elimination. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9644118-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3065166-A1 |
priorityDate |
2010-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |