Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_246a08bd416fe63ea8cc2483d2ce50db http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_754ec4107af54b28a149437061d82d92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ce030bd7e3ae0e400240548f408656e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_070f807e0706e3117dbda32c66c5c7cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9733c90c3036aa706d7ef1427ccb4a53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a415b486e5457df2451009309ead0e36 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2430-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-3683 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-3608 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61P19-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F2-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-36 |
filingDate |
2007-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d75f9d0b4ebfeba14288a5a9b0af595f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c92cca7ee3b95031d93ad99ba74eee1a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86c65b346072b633324b07683c7ba1c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b99aacdf70a10a12d86ac62d9a44e268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef2e742b2b62503a1720efa93a82ece7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ce25e49f4d5dcf0ea846c9ff5a8462c |
publicationDate |
2007-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2007168030-A1 |
titleOfInvention |
Osteoimplant and Method for Making Same |
abstract |
A method of manufacturing an osteoinductive osteoimplant is provided which comprises the steps of: demineralizing part or all of at least one surface of a monolithic section of cortical bone to a depth of at least about 100 microns; and, configuring the monolithic section of cortical bone to provide an osteoimplant possessing an outer surface possessing at least one demineralized zone and a non-demineralized zone. An implant produced according to the above method demonstrates improved osteoinduction without producing any clinically significant reduction of strength in critical regions of the osteoimplant. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8221500-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8740987-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8906110-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-RE42208-E http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8292968-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-RE43258-E http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10077420-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7815926-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7901457-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8435551-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7959683-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7837740-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9701940-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7879103-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014031937-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11555172-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9585764-B2 |
priorityDate |
1999-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |