abstract |
A method for low temperature bumping is disclosed. A resin capable of being cross-linked by free-radical or cationic polymerization at low temperature is provided. Electrically conductive particles are then added to the resin to form a mixture. The mixture is then activated by heat or exposure to light to polymerize the mixture. In an alternative embodiment, a vinyl ether resin is used, to which electrically conductive particles are added. The mixture is polymerized by exposure to light. |