abstract |
Embodiments of the invention address several issues and problems associated with etching of dielectric materials for BEOL applications. According to one embodiment, the method includes providing a patterned substrate containing a dielectric material, exposing the substrate to a gas phase plasma to functionalize a surface of the dielectric material, exposing the substrate to a silanizing reagent that reacts with the functionalized surface of the dielectric material to form a dielectric film, and sequentially repeating the exposing steps at least once to increase a thickness of the dielectric film. According to one embodiment, the dielectric material may be a porous low-k material, and the dielectric film seals the pores on a surface of the porous low-k material. |