abstract |
α-sialon phosphor particles containing Eu. At least one minute recess is formed on the surface of the α-sialon phosphor particles. The α-sialon phosphor particles are preferably produced by passing through a mixing step of raw materials, a heating step, a pulverizing step and an acid treatment step. |