abstract |
(2) a melt index (MI, 190 DEG C, under a load condition of 2.16 kg) of from 0.1 g / 10 min to 15 g / m < (3) the density and the melting temperature Tm satisfy the following relationship: Tm = a × db (2350 <a <2500, 1900 <b <2100) (Shore A) ratio (hardness / Tm) of from 1.0 to 1.3, wherein the olefinic polymer according to the present invention exhibits excellent anti-blocking properties since it has an improved hardness as a low density olefinic polymer . |