abstract |
The present invention relates to an improved coating material based on a cross-linked, RMA system with the help of conventional Michael addition. The coating material comprises at least one or more CH acidic compound A, 4 to 40 wt.% Of one or more vinylic carbonyl compounds B, 1.5 to 15 wt.% Of one By weight of at least one light stabilizer, up to 20% by weight of an open time extender, up to 20% by weight of at least one pot life extender, up to 70% By weight of one or more inorganic and / or organic pigments, and from 0.1 to 40% by weight of one or more anti-corrosive agents. The invention also relates to produced coatings, in particular to single layer top coats, and to coated parts, in particular agricultural machinery and construction machinery, for example for automobile body parts, tools or parts for attachment parts. |