Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2667-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02C2202-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2629-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0034 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00413 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00442 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02C7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00644 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0048 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-02 |
filingDate |
2016-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2018-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101878116-B1 |
titleOfInvention |
PLASTIC LENS MANUFACTURING METHOD, FILM POSITIONING METHOD |
abstract |
A method of manufacturing a plastic lens according to the present invention comprises the steps of: stacking a first curable composition on a corresponding formation surface of a first mold substrate having a formation surface for forming a lens surface; A step of separating the first mold substrate and the film from each other by a predetermined distance through a first curable composition layer formed by pressing and spreading over the entire surface of the first mold substrate; A step of disposing the second mold substrate so as to face the outer edge of the second mold substrate having the forming surface for forming the surface of the first mold substrate with a fixing member so as to face the film with a predetermined distance therebetween, Injecting a second curable composition into the gap of the second mold substrate; and curing the first curable composition layer and the injected second curable composition , Forming a base layer on both sides of the film, and removing the fixing member, the first mold substrate and the second mold substrate to take out the plastic lens. |