http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101309149-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 |
filingDate | 2011-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101309149-B1 |
titleOfInvention | Manufacturing method of positive electrode active material for lithium secondary battery and lithium secondary battery using same |
abstract | A method of manufacturing a cathode active material for a lithium secondary battery and a lithium secondary battery using the same, comprising: a) mixing a composite metal precursor and a lithium compound; b) calcining the mixture of step a) to produce a cathode active material; c) mixing the positive electrode active material, the carbon coating material and the solvent prepared in step b); And d) heat treating the mixture of step c) to obtain a cathode active material coated on the surface of the carbon coating material, wherein the content of the carbon coating material of step a) is a complex of step a). When the total amount of the metal precursor, the lithium compound and the carbon coating material is 100% by weight, 1 to 30% by weight, the firing temperature of step b) is 400 to 900 ° C, and the cathode active material obtained in step d). May provide a method for producing a cathode active material for a lithium secondary battery, which is represented by Formula 1 below. [Formula 1] Li a MeO 2 The definition for Formula 1 is present in the present specification. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9960419-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10862113-B2 |
priorityDate | 2011-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 152.