http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101250982-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-0285 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-107 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-0026 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-00 |
filingDate | 2011-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101250982-B1 |
titleOfInvention | Metal electrode pattern manufacturing method and manufacturing apparatus |
abstract | Metal electrode pattern manufacturing method of the present invention, the coating step of slot die coating the organometallic compound ink on the substrate; A preheating step of heating the coated substrate; A pattern forming step of irradiating a laser beam from a single laser source on the heated substrate through a laser scanner to form a pattern; A cleaning step of cleaning the substrate on which a pattern is formed; And a heating step after heating the washed substrate. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160064815-A |
priorityDate | 2011-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 22.