http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2021124865-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2379-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-281 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34 |
filingDate | 2020-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2021124865-A1 |
titleOfInvention | Laminate |
abstract | Provided is a laminate in which the polyimide film is stably peeled off from the protective film even after storage, and the adhesiveness of the polyimide film is not deteriorated, plasticized, or whitened. Using a protective film in which the solvent-extracted low molecular weight component is 0.03 to 3.0% by mass, the contact transfer amount of the solvent-extracted low molecular weight component to the polyimide film surface in the protective film after storage under load is 0.5 to 0.5. A laminate that achieves the task is obtained by limiting the amount to 50 mg / m2. |
priorityDate | 2019-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |