abstract |
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having a small change in color tone at the time of high-temperature melt processing, a good color tone of a molded article, and excellent flame retardancy. SOLUTION: (B) 1 to 50 parts by weight of a bromine compound (B) and 0 to 25 parts by weight of an inorganic flame retardant aid per 100 parts by weight of a thermoplastic resin. And the content of impurities derived from specific moisture is 0.1 to 1 mol of the specific bromine compound. A flame-retardant resin composition of not more than 02 mol. |