classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-283 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 |
filingDate | 1994-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1997-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09503531-A |
titleOfInvention | Method for producing low density porous crosslinked polymeric material |
abstract | (57) [Summary]nIn a method for producing a low density porous crosslinked polymeric material by polymerizing a water-in-oil type high discontinuous phase emulsion, the curing time of the monomers in the emulsion is By activating the above-mentioned monomers, the length can be shortened without adversely affecting the properties of the polymer. All or part of the monomers are activated by the presence of the activation initiator or the free-radical generating radiation source from about 5% to about 95% of the time effective to form a solid. The activated monomers, and optionally additional monomers, then form a high discontinuous phase emulsion of the water-in-oil type, the activated monomers containing other monomers. Added to water-in-oil type high discontinuous phase emulsions. The emulsion containing the activated monomers is cured. The method provides an improved method for incorporating volatile monomers into porous polymeric materials. The curing time is further shortened by carrying out the polymerization and crosslinking in the presence of alkylperoxycarbonate or alkylperoxycarboxylate polymerization initiators branched in the 1- and / or α-positions. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002128811-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6630519-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004517969-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0234797-A1 |
priorityDate | 1993-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |