http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08188921-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 |
filingDate | 1994-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3683d89377aecef92f5e546acd0d9664 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b455ba17262032fd51491b09c3f0cd22 |
publicationDate | 1996-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08188921-A |
titleOfInvention | Polyester fiber having improved weather resistance, method for producing the same, and fiber product using the fiber |
abstract | (57) [Summary] [Structure] A polyester fiber containing an ultraviolet absorber in an amount of 3.0% by weight or less based on the total weight of the fiber, and the ultraviolet absorber corresponds to 25% of the single fiber cross-sectional area. A polyester fiber having improved weather resistance, which is contained in the surface layer portion in a concentration of more than 3.0% by weight, and a fiber product using the same. After immersing the polyester fiber in an aqueous dispersion of the ultraviolet absorber, the nip roller squeezes it so that the amount of the ultraviolet absorber attached to the solid content is 3.0% by weight or less, and after drying, 200 to Weather resistance characterized by containing the ultraviolet absorber in a concentration of more than 3.0% by weight in the surface layer portion corresponding to 25% of the single fiber cross-sectional area of the polyester fiber by heat treatment at 220 ° C. Of improved polyester fiber. [Effect] The weather resistance of the polyester fiber used outdoors, which is exposed to intense ultraviolet rays for a long time, is greatly improved, and the strength retention is also excellent. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008102822-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100493111-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008123504-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009022736-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009123141-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009136624-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009123142-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1397247-A4 |
priorityDate | 1994-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.