http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0718051-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-00 |
filingDate | 1993-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67a7ab470c7b3f1dc0bda838b3a65360 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_919e0b68994a85d3e97abe7424b59a04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac1565d2ecc9734f50216a3a657ce0e1 |
publicationDate | 1995-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0718051-A |
titleOfInvention | Moisture-curable polyurethane surface finish containing polyaldimines |
abstract | (57) [Summary] [Structure] Moisture curability containing 57 parts by weight of dialdimine represented by the formula, 700 parts by weight of polyurethane prepolymer having an isocyanate group, 600 parts by weight of calcium carbonate as a filler and 50 parts by weight of hydrophobic silica as a thixotropic agent as main components Polyurethane surface finish material. [Effect] This surface finish material has excellent storage stability in a closed container. Also, once opened, it reacts with moisture in the air and rapidly hardens. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016513142-A |
priorityDate | 1993-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 101.