Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2973 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2969 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-253 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-605 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-60 |
filingDate |
1991-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2fe58c2deda33f29de64c2aba49b91a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b308126fb07035f9f4ec243de8db852 |
publicationDate |
1993-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05163610-A |
titleOfInvention |
Aromatic polyamide flat fiber |
abstract |
(57) [Summary] [Object] It is an object of the present invention to provide an aromatic polyamide flat fiber having a low coefficient of friction between fibers, a low stress strain during yarn twisting, and a high cord strength utilization rate. [Structure] Aromatic polyamide flat fiber strength characterized by fiber flatness of 1.5 or more and 5 or less, single yarn fineness of 1 denier or more and less than 50 denier, and mechanical properties in the following range: 18 g / de Elongation: 3.5% or more Initial modulus: 450 g / de or more |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003221729-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6033778-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003049388-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9744510-A1 |
priorityDate |
1991-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |