http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6366888-B1
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-16 |
filingDate | 2018-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-6366888-B1 |
titleOfInvention | Ethylene polymer, stretched molded product, microporous membrane, and fiber |
abstract | In the present invention, the viscosity average molecular weight is 100 × 10 4 or more and 1,000 × 10 4 or less, and the ratio of the isothermal crystallization time of 125 ° C. to 123 ° C. determined by specific isothermal crystallization time measurement conditions is 3. Provided is an ethylene polymer having a crystallinity of 5 to 10.0 and a crystallinity obtained from a differential scanning calorimeter (DSC) of 40% to 75%. |
priorityDate | 2017-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links