Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2305-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B43-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate |
2018-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5af5ceba2ccda0dfb0fde228996a62c |
publicationDate |
2019-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2019159200-A |
titleOfInvention |
Method for producing optical laminate and method for producing optical laminate with adhesive layer |
abstract |
An optical laminated body in which reverse curling is suppressed and an optical laminated body with an adhesive layer can be produced. A method of manufacturing an optical laminate in which an optical film, a first adhesive cured layer, a first liquid crystal layer, an adhesive layer, and a second liquid crystal layer are laminated in this order is provided via the first adhesive cured layer. The step of laminating the optical film on the first liquid crystal layer side of the first liquid crystal layer with the base material layer to obtain the first liquid crystal layer laminate with the base material layer, and the first liquid crystal layer laminate with the base material layer first A step of peeling the base material layer to obtain a first liquid crystal layer laminate, a first exposed surface side of the first liquid crystal layer laminate exposed by peeling the first base material layer, and a second liquid crystal layer Laminating the first liquid crystal layer laminate and the second liquid crystal layer with the base material layer so as to face each other through the adhesive layer, and obtaining a second liquid crystal layer laminate. The adhesive layer is a first adhesive layer or a second adhesive cured layer. [Selection] Figure 4 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021117569-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021092770-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023037715-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022049847-A1 |
priorityDate |
2018-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |