http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019099654-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 |
filingDate | 2017-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bab50d44ddc6b5a52c1cba288925a338 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b460e4bd020ffc68b54ba9d154f8865 |
publicationDate | 2019-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019099654-A |
titleOfInvention | Polyoxymethylene resin molded product |
abstract | An object of the present invention is to provide a polyoxymethylene resin molded article and a polyoxymethylene resin composition which have a low odor, a small amount of foreign matter generation even when continuous molding is performed, and high grease resistance. A total area corresponding to the surface area of one rectangular solid of 60 mm × 60 mm × 3 mm containing 100 parts by mass of a polyoxymethylene resin and 0.1 to 0.5 parts by mass of an amide compound having a melting point of 300 ° C. or higher. The amount of acetic acid extracted from one or more molded articles having a surface area into 150 g of water coexisting in an environment at 80 ° C. for 15 days is 80 mass ppm or less based on the total mass of the molded articles A molded article molded into a rectangular solid of 60 mm × 60 mm × 3 mm containing a methylene resin molded article and 100 parts by mass of a polyoxymethylene resin and 0.1 to 0.5 parts by mass of an amide compound having a melting point of 300 ° C. or more A polyoxymethylene resin composition wherein the amount of acetic acid extracted in 150 g of water coexisting in an environment of 1 to 80 ° C. and 15 days is 80 mass ppm or less based on the total mass of the molded article. 【Selection chart】 None |