Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate |
2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b460e4bd020ffc68b54ba9d154f8865 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bab50d44ddc6b5a52c1cba288925a338 |
publicationDate |
2017-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2017082098-A |
titleOfInvention |
Composite parts, polyoxymethylene resin parts, and resin compositions |
abstract |
The present invention provides a composite part that retains its appearance and has excellent durability operability when used in a high temperature and high humidity environment. The amount of acetic acid extracted into 150 g of water containing a metal part M and a polyoxymethylene resin part P and coexisting in an environment at 80 ° C. for 15 days is the mass of the polyoxymethylene resin part P. A composite part having a mass of 100 mass ppm or less. [Selection] Figure 7 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020100713-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11661511-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7204474-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11555111-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019099654-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020129663-A1 |
priorityDate |
2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |