abstract |
As raw materials, base phase change resin 3-10%, synthetic rubber 1-5%, thickening resin 5-10%, antioxidant 0-1%, coupling agent 0-5% by weight percentage And a rubber-modified phase change heat conductive material containing 69 to 85% of heat conductive particles and a method for producing the same. The rubber-modified phase change heat conductive material has improved heat conductivity. [Selection figure] None |