abstract |
An object of the present invention is to provide a toner capable of suppressing discharge adhesion after being fixed at low temperature in LBP speeded up more than before. A toner having toner particles containing at least a charge control agent and a crystalline resin, which is held at 80 ° C. for 5 minutes and then cooled to 60 ° C. at 750 ° C./min in endothermic measurement of the toner, The time t1 / 2 until 50% of the area of the exothermic peak when held at 60 ° C. is 0.03 minutes or more and 0.32 minutes or less, and the charge control agent is a compound of the formula [1]. 【Selection chart】 None |