http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017141368-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3d32c1a141872565553b73d633c8c166 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 |
filingDate | 2016-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0d4d7ef75885143d5acc5b73221910d2 |
publicationDate | 2017-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017141368-A |
titleOfInvention | Method for producing mixed latex in which pigment and latex are mixed |
abstract | The present invention relates to a mixed latex in which a mixed latex is produced by a first step for base formation and a second step for final treatment, and the produced mixed latex is mixed with a pigment that can be used as a paint and latex. The purpose is to realize a manufacturing method. Therefore, in a method for producing a mixed latex in which a coloring pigment is mixed with a latex for forming a film, the method comprises a first step for base formation and a second step for final treatment. Puts a predetermined amount of latex into the stirring vessel, adds water, vulcanization accelerator, stabilizer and pH adjuster to the latex, and stirs the ammonia odor while stirring in the stirring vessel for the first predetermined time. In the second step after the first step, a coloring pigment, a fragrance, a thickener, and an anti-aging agent are added to the base latex in the stirring vessel, and the second step is performed in the stirring vessel. A mixed latex is produced by stirring for a predetermined time. [Selection] Figure 1 |
priorityDate | 2016-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.