http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017097352-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c97f90ab12b35b650d5fd039ed7a41a5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-14 |
filingDate | 2016-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fa6a01e20fc278a92710b5eb2308c3c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff98702b10b676936add9b683c4b543b |
publicationDate | 2017-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2017097352-A |
titleOfInvention | Optical film, method for producing the same, and polarizing plate using the same |
abstract | Provided are a zero retardation film capable of preventing the polarizing plate from being cracked when used for producing a polarizing plate, and a method for producing the same, even when the thickness is reduced. An optical film is configured such that, in a thin zero retardation film, the stress at break in either the longitudinal direction or the lateral direction is a predetermined value or more. Further, when the optical film is produced, when the original film is subjected to a stretching treatment, one of the stretching ratio in the longitudinal direction (MD direction) and the stretching ratio in the width direction (TD direction) is 1.01 times the other. An anisotropic stretching process as described above is performed. [Selection figure] None |
priorityDate | 2016-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links