http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015178580-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-00 |
filingDate | 2014-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4813dffdd66aeb6d5d69d1c98f12ba6b |
publicationDate | 2015-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015178580-A |
titleOfInvention | Resin composition and use thereof |
abstract | PROBLEM TO BE SOLVED: To provide a resin composition suitable for a light reflector which is not deformed even under a high temperature environment and whose light reflectance is not lowered. I will provide a. (A) To 100 parts by weight of a crystalline cyclic olefin ring-opening polymer hydrogenated product having a repeating unit derived from a polycyclic norbornene monomer having three or more rings, (B) aspect ratio of 2 A resin composition comprising 5 to 100 parts by weight of ~ 100 whiskers and 5 to 20 parts of (C) a white pigment is molded to obtain a light reflector such as an LED. The obtained light reflector maintains a high reflectance even after the heat resistance test and has excellent heat distortion resistance. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022034888-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20230049082-A |
priorityDate | 2014-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 247.