http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015096628-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b7344709565cf9669f58790095b5dce6 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-02 |
filingDate | 2013-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_840a3235b6a32c06f73fe303ab0fd6a9 |
publicationDate | 2015-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2015096628-A |
titleOfInvention | Method for producing scaly fine powder |
abstract | PROBLEM TO BE SOLVED: To produce a scaly fine powder capable of recovering and reusing a substrate and a release layer, and obtaining a high-purity scaly powder with high yield and good productivity. I will provide a. SOLUTION: A polymer film is used as a base material, an ionic liquid having a melting point of 50 ° C. or higher and 150 ° C. or lower is provided on the surface of the base material, and then a thin film of metal or metal compound is formed on the surface of the ionic liquid. Laminating step of obtaining a laminate, heating the laminate above the melting point of the ionic liquid, peeling the ionic liquid and the thin film from the substrate, and the ionic liquid A method for producing a scaly fine powder, comprising: a separation and recovery step of separating the thin film and recovering the thin film. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6214720-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107344239-A |
priorityDate | 2013-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 87.