Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate |
2013-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_659e58b875c2c5425e91a25abe107e76 |
publicationDate |
2014-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2014205814-A |
titleOfInvention |
Diisopropyl fumarate-cinnamate-bismaleimide copolymer resin and method for producing the same |
abstract |
PROBLEM TO BE SOLVED: To provide a novel high molecular weight diisopropyl fumarate-cinnamic acid ester-bismaleimide copolymer resin having excellent toughness even when formed into a film, and a method for efficiently producing the same. A diisopropyl fumarate-cinnamate-bismaleimide copolymer resin comprising a diisopropyl fumarate residue unit, a cinnamic acid ester residue unit having an alkyl group having 1 to 6 carbon atoms, and a bismaleimide residue unit. . [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016108544-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016084747-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016145289-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016145288-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016098371-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7040175-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016145291-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016145290-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016094576-A |
priorityDate |
2013-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |