http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014103003-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bd0cdbc5c67cf4957ed83c89140748e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-30 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0402 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-52 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 |
filingDate | 2012-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_07de226bc5bb1c290a7224d90723693e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ada04b9e027573f49d6d7bfdd523d197 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e535576745d7d0c5b22eb4fef1a1a04f |
publicationDate | 2014-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2014103003-A |
titleOfInvention | Coated nickel hydroxide powder for positive electrode active material of alkaline secondary battery and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a coated nickel hydroxide powder capable of improving the dispersibility when it is made into a paste and suppressing agglomeration, and capable of high-density filling into a three-dimensional metal porous body when producing a positive electrode for an alkaline secondary battery. SOLUTION: The pH of a suspension obtained by adding 10 ml of water to 10 g of coated nickel hydroxide powder, which is a coated nickel hydroxide powder in which the surface of nickel hydroxide particles is coated with a coating layer of a cobalt compound. ) Is 10.2 or more. Therefore, the amount of ammonium ions eluted in the suspension obtained by adding 10 ml of water to 10 g of the coated nickel hydroxide powder in the washing step of the coated nickel hydroxide powder obtained by obtaining the crystallization step and the coating step is as follows. Wash until 0.35 mmol / l or less. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7070250-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020033213-A |
priorityDate | 2012-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links