Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_063a1b324005ddc15e16e7529c6258c4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48247 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-62 |
filingDate |
2010-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75a86158b9af6ca5ec857f00022f6cd7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c0ddd2b3777b0a3ce4c05b200d87266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3925e555cc98dbd50dca393768d3c84 |
publicationDate |
2011-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2011222680-A |
titleOfInvention |
Lead frame for optical semiconductor device and method for manufacturing lead frame for optical semiconductor device |
abstract |
It is an object of the present invention to ensure adhesion and to ensure luminous efficiency. SOLUTION: A nickel or nickel alloy plating film 3 and a silver alloy plating film 4a containing antimony are laminated on a metal material 2, and silver plating is performed using a low cyan silver plating solution on at least a region where the reflector 5 is formed. By forming the film 4b, it is possible to ensure adhesion and to ensure luminous efficiency. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021153243-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014204046-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016006898-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015140469-A |
priorityDate |
2010-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |