http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011131391-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2009-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10052a7cec969df15c90c04c419aa465 |
publicationDate | 2011-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011131391-A |
titleOfInvention | Biaxially oriented polyester film for vapor deposition |
abstract | 【Task】 Provided are a biaxially oriented polyester film for vapor deposition and a gas barrier film having excellent oxygen barrier performance, water vapor barrier performance, and water-resistant adhesion. [Solution] The above-mentioned problem is a biaxially oriented polyester film for vapor deposition comprising an anchor coat layer made of a polyurethane resin (A) on at least one side of a polyester film, A minute endothermic peak before crystal melting obtained by differential scanning calorimetry measurement of the biaxially oriented polyester film for vapor deposition is at 180 ° C. or higher and 220 ° C. or lower, and the polyurethane resin (A) is a polyisocyanate component (A1), A resin comprising a polyol component (A2), wherein the polyisocyanate component (A1) contains an araliphatic diisocyanate (A1A) and / or an alicyclic diisocyanate (A1B), and the polyol component (A2) By the biaxially oriented polyester film for vapor deposition containing at least polyhydroxyalkanoic acid (A2C) and further containing an alkane polyol having 2 to 6 carbon atoms (A2A) and / or a polyoxyalkylene glycol having 2 to 6 carbon atoms (A2B) Achieved. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012039259-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015174270-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021060004-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016143889-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5597716-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114423601-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10434751-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016143889-A1 |
priorityDate | 2009-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |