http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010107680-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-42 |
filingDate | 2008-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fec3a7446e622db7575824c17263fb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c15ac9b5bff9f5d990a6f07f7b9c058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2324f749355af10bc040816f072a1359 |
publicationDate | 2010-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2010107680-A |
titleOfInvention | Optical element and optical element manufacturing method |
abstract | An optical system having a light resistance and optical characteristics by having a bonding film whose refractive index changes in the thickness direction, and firmly bonding two optical components with high dimensional accuracy via the bonding film. To provide an element and a method of manufacturing an optical element that can easily manufacture such an optical element. A laminated optical element includes a first optical component and a second optical component, and a bonding film is formed on the surface of the first optical component by plasma polymerization. The first step, the second step in which energy is applied to the bonding film 3 by exposing the bonding film 3 to plasma and the adhesiveness is expressed, and the first optical component 2 and the first step through the bonding film 3 2 is bonded to the optical component 4 to obtain the laminated optical element 5, and the refraction of the bonding film 3 is performed by gradually changing the film forming conditions in the plasma polymerization method. The refractive index is changed so as to connect the refractive index of the first optical component 2 and the refractive index of the second optical component 4. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016200739-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013119796-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014503683-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108369984-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10892385-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015511332-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9705056-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11442349-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9259905-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023281792-A1 |
priorityDate | 2008-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.