abstract |
The present invention provides a method for producing a pearly luster composition having high whiteness while maintaining strong pearly luster and having excellent dispersion stability. SOLUTION: It contains a fatty acid glycol ester, a surfactant, and water, and further includes (1) fatty acid, (2) aliphatic alcohol, (3) fatty acid monoglyceride, and (4) as a crystallization additive. A method for producing a pearly luster composition comprising any one selected from the group consisting of aliphatic ethers, comprising a fatty acid glycol ester, a surfactant, water, and a crystallization additive. A method for producing a pearly luster composition, comprising a step of cooling the liquid, wherein the representative heat removal rate per unit mass during crystallization in this cooling step is 9 to 36 [W / kg]. [Selection figure] None |