http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009248422-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K69-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 |
filingDate | 2008-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_94be5f72084972a29e63caa196876719 |
publicationDate | 2009-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009248422-A |
titleOfInvention | Method of molding aromatic polycarbonate resin molded article and molded article thereof |
abstract | An object of the present invention is to provide a method for molding an aromatic polycarbonate resin molded article free from burns in injection molding and excellent in transparency, and a molded article thereof. A method of injection molding an aromatic polycarbonate resin composition (component A) using an injection molding machine, wherein the compression ratio of the screw in the injection molding machine is in the range of 1.4 to 2.0. And the ratio (C / L) of the length (C) of a compression zone and screw full length (L) exists in the range of 0.3-0.7, The injection molding method characterized by the above-mentioned. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103566862-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103566862-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104129049-A |
priorityDate | 2008-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 218.