http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009186482-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a47f505748653ebbd8cd8d9a0cc749b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N27-409 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-90 |
filingDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de2bd9da7fdbb8af57261dc566172e9a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98d1d0e905b80a8bf45c404b28e6ac53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d70f93eba0dea8f8cb98cdaf4b5317cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6256c3be004a88b022dd4507ddbadf1 |
publicationDate | 2009-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009186482-A |
titleOfInvention | Electrode for solid electrolyte and method for producing the same |
abstract | An object of the present invention is to focus on ruthenium oxide as an electrode material for a solid electrolyte, and to produce a solid electrolyte electrode capable of forming an electrode having a fine structure capable of maximizing and maintaining the original physical properties of ruthenium oxide. Is to provide. A method for producing a solid electrolyte electrode according to the present invention is obtained by obtaining a crude raw material of dipivaloylmethanate ruthenium, purifying it by a column chromatography method, and further heating and vaporizing the raw material purified by sublimation. A process, a step of stirring a raw material vaporized using an inert gas as a carrier gas together with oxygen gas with a mixer, and then transporting the raw material onto a solid electrolyte substrate; And a step of forming a ruthenium oxide electrode, wherein the ruthenium oxide electrode is composed of particles having a uniform particle diameter so that the microstructure does not change even when heat-treated at 850 ° C. for 8 hours. And [Selection] Figure 1 |
priorityDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |